Magnet trading · Nike Industrial Trading[email protected]WhatsApp +852 4607 0157

Magnet materials and specifications

Sintered NdFeB Processing, Temperature and Shape Constraints

Sintering densifies an aligned NdFeB compact. The temperature and hold time depend on the powder and part. Read the full heat-treatment sequence, then check shrinkage and finished dimensions in the relevant directions.

Nike Industrial Trading Published 20 November 2026

Furnace chamber containing a rectangular compact, with ring and slender-cylinder parts shown beside it
Process schematic showing a sintering chamber and two finished shape concepts.

Sintering, heat treatment and finishing have different jobs

In conventional sintered NdFeB production, a magnetic field aligns the powder before or during pressing. Pressing forms a green compact. During sintering, a rare-earth-rich liquid phase assists densification and the compact shrinks. Heat treatment after sintering adjusts the grain boundary structure and can change intrinsic coercivity. Machining brings the part to its drawing dimensions before the relevant finishing, magnetizing and inspection steps. [1] [2] [3]

Use density to assess densification and measure along defined axes to track shrinkage. If a finished part misses a fit dimension, check the as-sintered blank against its machining allowance. Then check how much material was removed and compare the finished part with the drawing. Confirm magnetic acceptance after the specified heat treatment and magnetization. The manufacturing overview covers powder preparation and the rest of the production route. [1] [2]

Read sintering temperature with composition and hold time

A temperature by itself cannot describe a sintering cycle. The starting powder, atmosphere, hold and later thermal treatment all affect the result. Use a supplier’s qualified process for its own alloy and part geometry. For acceptance, ask which zone or sensor the temperature describes and how the supplier verifies density, directional shrinkage and final magnetic properties. [1] [2] [4] [5]

Published sintering and heat-treatment examples
Material or studySintering conditionHow to read the example
Ce-containing rectangular specimens1,045 °C in vacuum for 6 hFollowed by 780 °C for 3 h and 640 °C for 6 h. Alignment field varied within the study, and shrinkage varied by direction. [1]
DyF3-doped NdFeB specimens1,050, 1,060 and 1,070 °C for 4 h in separate trialsWith composition and hold time fixed, the 1,050 °C specimen reached a reported coercivity of 35.1 kOe after the study’s post-sinter heat treatment. Compare the temperatures within this series. [4]
EP3827916B1 example 21,060 °C in vacuum for 12 hFollowed by 850 °C for 3 h and 480 °C for 3 h. The patent applies to its own powder and process. [3]

Published sintering and heat-treatment examples

Ce-containing rectangular specimens

Sintering condition
1,045 °C in vacuum for 6 h
How to read the example
Followed by 780 °C for 3 h and 640 °C for 6 h. Alignment field varied within the study, and shrinkage varied by direction. [1]

DyF3-doped NdFeB specimens

Sintering condition
1,050, 1,060 and 1,070 °C for 4 h in separate trials
How to read the example
With composition and hold time fixed, the 1,050 °C specimen reached a reported coercivity of 35.1 kOe after the study’s post-sinter heat treatment. Compare the temperatures within this series. [4]

EP3827916B1 example 2

Sintering condition
1,060 °C in vacuum for 12 h
How to read the example
Followed by 850 °C for 3 h and 480 °C for 3 h. The patent applies to its own powder and process. [3]
Hold stages from the published Ce-containing rectangular specimen. Heating and cooling ramps and elapsed time between stages are outside the diagram.

Inspect a radial ring and a slender cylinder differently

Radially oriented ring. In the route described in US7524453B2, tooling creates a radial alignment field in the ring cavity before the powder compact is sintered. Cooling can build residual stress when thermal expansion differs along and across the local material orientation. Inspect the bore for cracks and check outside diameter, bore, roundness and fit before measuring the finished pole pattern at the specified gap. A radial material orientation and a particular multipole pattern are separate drawing requirements. [6] [7] See the ring drawing guide.

Slender cylinder. CN115301946B gives a target of Ø5 × 25 mm and a designed sintered blank of Ø5.4 × 25.6 mm. The 0.4 mm difference is on the diameter and the 0.6 mm difference is on the overall length. These are the allowances in one patent example. For a production drawing, agree where to check diameter along the length, how to measure straightness, and what stock remains for grinding. Ask for as-sintered and finished measurements from the proposed process. [8] [9] See the cylinder specification guide.

Example inspection locations on a radial ring and a slender cylinder. Choose the datum and actual tolerances from the finished drawing.

Details to send for a sintered part

Finished drawing, revision, units and critical tolerances:
Ring or cylinder measurement stations and reference surfaces:
Magnetic axis, pole pattern, working gap and field requirement:
Grade or magnetic-property limits and magnet temperature:
Surface finish, inspection methods and acceptance limits:
Sample and production quantity:

Technical sources

Read each source with its stated material, test conditions and publication scope.

  1. Alignment and shrinkage in sintered NdFeBExperimental procedure and Figure 4. Ce-containing rectangular specimens.
  2. Li et al., coercivity of NdFeB permanent magnetsSection 2 explains liquid-phase sintering and post-sinter annealing.
  3. EP3827916B1, sintered NdFeB manufacturingExample 2, paragraphs 0052–0053.
  4. Effect of sintering conditions on DyF₃-doped NdFeBExperimental Procedure and Figures 1–2. Temperature comparisons hold doped composition and time constant.
  5. Tomše et al., thermal-radiation-assisted sinteringExperimental parameters distinguish crucible temperature and specimen response.
  6. US7524453B2, forming and sintering radially oriented ringsDescription and Figures 4–5 distinguish powder orientation, compaction and sintering.
  7. EP1308970B1, radial anisotropic sintered magnet productionDescription of cooling stresses and cracking in radial rings.
  8. CN115301946B, cylindrical sintered blank shapeExample 1 and Figures 4–5. Example dimensions describe this patent.
  9. CN103426621B, directional shrinkage of sintered NdFeBTable 1 and its discussion are specific to the disclosed materials and process.

Have a ring or cylinder drawing?

Identify the critical finished dimensions and how the magnet will be checked.