At what temperature does a PMSM magnet demagnetize?
There is no single demagnetization temperature for NdFeB in a permanent magnet synchronous motor (PMSM). The onset of irreversible loss depends on the grade's hot demagnetization curve and the field acting on each part of the magnet. A drive can see less flux at elevated temperature and recover on cooling. If a local region passes the relevant knee, some loss can remain after the reverse field is removed and the rotor cools.[1] [2]
Use the curve for the proposed material and magnet temperature. A suffix or maximum working-temperature entry cannot represent the rotor geometry, fault current or allowed loss. See the general temperature guide for the distinction between reversible and irreversible loss.
Compare the weakest region with the hot curve
A second-quadrant curve shows what happens as a field opposes the magnetization. A simple load line can explain the trend, but an interior rotor bridge, air gap, leakage path and armature current make the field nonuniform. Check the region and time with the worst margin. A rotor-average field can hide a small demagnetized region. For oblique fields, use a material model appropriate to the magnet and field direction.[2] [3] [4]
Define the knee by the curve and agreed loss criterion used in the assessment. Intrinsic coercivity HcJ is the reverse-field magnitude at which intrinsic polarization reaches zero. The permissible field in an assembly depends on its loss criterion and the full curve. Specify the hottest relevant magnet region. A winding or coolant temperature is useful only when a model or measurement relates it to the magnet temperature.[1] [2] [5] [10]
Normal duty, field weakening and fault cases
| Case | Why it matters | Useful input |
|---|---|---|
| Continuous hot load | Rotor heating shifts the material curve while armature current changes the local field. | Magnet temperature map or justified bounds, current, speed and cooling condition |
| High-speed field weakening | Negative d-axis current under the usual convention opposes the magnet flux. Current limits and rotor geometry determine the margin. | Id/Iq envelope and sign convention, speed, hot curves and magnet geometry |
| Overload, short circuit or inverter fault | A transient can produce an opposing field different from steady-state operation. | Initial temperature, speed and current, fault topology, time history and clearing behaviour |
Cases to include in a rotor demagnetization review
Continuous hot load
- Why it matters
- Rotor heating shifts the material curve while armature current changes the local field.
- Useful input
- Magnet temperature map or justified bounds, current, speed and cooling condition
High-speed field weakening
- Why it matters
- Negative d-axis current under the usual convention opposes the magnet flux. Current limits and rotor geometry determine the margin.
- Useful input
- Id/Iq envelope and sign convention, speed, hot curves and magnet geometry
Overload, short circuit or inverter fault
- Why it matters
- A transient can produce an opposing field different from steady-state operation.
- Useful input
- Initial temperature, speed and current, fault topology, time history and clearing behaviour
The fault case belongs to the specific machine and inverter. An open-end five-phase drive study modelled local loss under a transistor short, with results depending on operating temperature and torque reference. A separate IPMSM comparison examined the demagnetization risk of active short-circuit current alongside the voltage risk of open-circuit turn-off. These studies show why the actual fault and circuit need to be modelled together.[6] [7]
Check residual change after the rotor cools
Use a baseline and a post-event no-load measurement at the same rotor temperature, speed and voltage definition. If speeds differ slightly and the same machine and measurement convention apply, compare the fundamental back-EMF per unit speed. A hot reading alone cannot separate temperature effects from residual loss. A global voltage comparison can miss small or spatially balanced loss, so define when a pole-resolved check is needed.[2] [8] [9]
Teaching example: at a fixed speed, a rotor gives 100 V RMS fundamental line-to-line before a duty cycle, 92 V while hot and 98 V after returning to the starting temperature. The hot change is 8% and the cooled change is 2%. Compare the cooled change with repeatability and the agreed acceptance limit. Neither number directly gives the percentage of magnet volume that has demagnetized.
In one published IPMSM experiment, researchers reduced the thickness of the magnets in one pole of a four-pole rotor to imitate radial demagnetization. In the case labelled R-5.0%, the total magnet-material volume across the rotor was 95.5% of the healthy rotor's total. At 1500 rpm the back-EMF-derived flux linkage was 0.2055 Wb versus 0.2157 Wb for the healthy motor. The result illustrates the method on that rig. Other rotors need their own comparison.[8]
Information for a rotor magnet review
Start with the assembly cross-section, current grade and hot or fault case that concerns you. A material comparison can clarify which curves and tolerances to request. The motor design team sets the electrical duty, magnetic margin and validation method.
Rotor layout, drawing revision and magnet dimensions: Material grade, orientation and available hot B–H / J–H curves: Magnet temperature or basis for its estimate: Current and speed envelope, fault case and duration: Permitted cooled flux loss, measurement method and quantity:
Related technical guides
Technical sources
Read each source with its stated material, test conditions and publication scope.
- NdFeB for high-temperature motor applications
- Uršič et al., temperature-dependent PMSM demagnetization model
- Zhang et al., coupled electromagnetic and thermal modelling
- Song et al., hybrid traction motor and Dy-free magnets
- N42SH data sheet and temperature curves
- Dos Santos Moraes et al., open-end winding transistor fault
- Ragazzo et al., turn-off comparison in traction IPMSMs
- Ishikawa et al., IPMSM failure diagnosis
- Jeong et al., trailing edge demagnetization experiment
- Zhang et al., IPMSM rotor temperature monitoring